| modulo |
ASTM |
| Asta |
B 335 |
| Piatto, foglio e striscia |
B 333, B 906 |
| Tubo e tubo senza saldatura |
B 622 |
| Tubo saldato |
B 619, B 775 |
| Tubo saldato |
B 626, B 751 |
| Raccordo per saldatura |
B 366 |
Composizione chimica
| % |
Ni |
Mo |
Fe |
Co |
Cr |
C |
Mn |
Si |
P |
S |
V |
| verbale |
equilibrio |
26.0 |
4.0 |
|
|
|
|
|
|
|
0.20 |
| max |
30.0 |
6.0 |
2.5 |
1.00 |
0.050 |
1.00 |
1.00 |
0.040 |
0.030 |
0.40 |
Proprietà fisiche
| Densità |
9.24 g / cm3 |
| Intervallo di fusione |
1330-1380 ℃ |
Caratteristiche: Hastelloy B has excellent resistance to reducing environments like sulfuric acid at moderate concentrations and other nonoxidizing acids. It also resists stress corrosion cracking induced by chlorides. Hastelloy B has poor resistance to oxidizing environments, therefore, it should not be used where ferric or cupric salts are present as these salts may cause rapid corrosion failure.
Applicazioni: Movimentazione dell'attrezzatura che riduce gli ambienti chimici; e l'industria dei processi chimici che coinvolge acidi cloridrico, solforico, fosforico e acetico.
|
|