Composizione chimica
% |
Fe |
Ni |
Cr |
C |
Si |
Mn |
P |
S |
Ti |
Mo |
V |
Al |
B |
verbale |
equilibrio |
24.0 |
13.5 |
|
|
|
|
|
1.90 |
1.00 |
0.10 |
|
0.0010 |
max |
27.0 |
16.0 |
0.08 |
1.00 |
2.00 |
0.040 |
0.030 |
2.35 |
1.50 |
0.50 |
0.35 |
0.010 |
Proprietà fisiche
Densità |
7.94 g / cm3 |
Intervallo di fusione |
1370-1430 ℃ |
Caratteristiche: Incoloy A-286 is an age-hardenable alloy which can withstand oxidation and retain good strength at temperatures up to about 700℃. It can be readily formed by standard processes for stainless steels and nickel alloys.