- Grade:
Cliquez pour envoyer un courriel Vendeur
Spécification, Chemical & Performance mécanique
Standard: EN10025-2
Steel grade : S275JR, S275J0, S275J2, S235JR, S235J0, S235J2
Classification : Non-alloy structural steel
Application : Non-alloy steel for structural purposes
This are common mild steel/carbon steel plate for structural, manufacturing plant, machinery, mining equipment , excavators, loader, bulldozers, crane, mining hydraulic supports, construction, power plant, sugar mill, palm oil mill, oil and gas, port equipments, fans, drilling rigs, power shovel and other structural parts. Heat analysis shall be used to determine the required chemical composition for carbon. Manganese, phosphorus, sulfur, silicon, and copper. Tensile strength, yield strength, and elongation shall be evaluated using tension test.
S275JR and its related series (S275J0, S275J2, S235JR, S235J0, S235J2) are very versatile common mild steel/carbon steel plate for multiple structural applications e.g. manufacturing plant, machinery, mining equipment and vehicles, excavators, loader, bulldozers, crane, mining hydraulic supports, construction, power plant, sugar mill, palm oil mill, oil and gas, port equipments, fans, drilling rigs, power shovel and other structural parts. Heat analysis shall be used to determine the required chemical composition for carbon. Manganese, phosphorus, sulfur, silicon, and copper. Tensile strength, yield strength, and elongation shall be evaluated using tension test.
S symbol for structural steel
275 indication of the min specified yield strength for thickness of under16mm.
JR symbol 20 temperature impact test.
Symbole J0 Test d'impact de température 0
Symbole J2 - Test d'impact de température 20
S275JR Chemical is max composition of product analysis:
|
Nominal thickness = < 40(mm) C max = 0.21 Nominal thickness = < 40 (mm) CEV max = 0.40 |
||||||
|
C |
Mn |
P |
S |
N |
Cu |
CEV |
|
max 0.22 |
max 1.5 |
max 0.04 |
max 0.04 |
max 0.012 |
max 0.55 |
max 0.42 |
S275JR mechanical properties steel.
|
Nominal thickness (mm) |
- 16 |
16-40 |
40-63 |
63-80 |
80-100 |
100-125 |
|
ReH - Minimum yield strength (MPa) |
275 |
265 |
255 |
245 |
235 |
225 |
|
Nominal thickness (mm) |
3 - 100 |
100 - 125 |
|
Rm - Tensile strength (MPa) |
410 - 560 |
400 - 540 |
C’est à tous ces cambodgiens que nous souhaitons apporter notre offre.
|
Nominal thickness (mm) |
3 - 40 |
40 - 63 |
63 - 100 |
100 - 125 |
|
A - Minimum elongation Lo = 5,65√ So (%) |
23 |
22 |
21 |
19 |
C’est à tous ces cambodgiens que nous souhaitons apporter notre offre.
|
Température |
-20 |
0 |
20 |
|
Notch impact test. Min. absorbed energy |
27 |
27 |
27 |
L'énergie d'impact minimale est l'énergie longitudinale
S275JR, S275J0 and S275J2 EN10025-2 standard min thickness 5mm up to max thickness 390mm.
We can exclusively produce steel plate thickness 5mm X width 2000mm X your choice of length.